CERAMIC COATED M.S. LANCING PIPES |
|
| |
| The practice lancing/purging in coreless induction furnace melting in EAF has been established for a very long time. Normally steel tubes are used for injecting ARGON, NITROGEN into the furnace. This results in the tubes melting at the tip at a very fast rate. Ceramic coating helps reduce this consumption by a great extent resulting in the following advantages: Longer lancing time without interruption, more effective use of the un-burnt gasses leaving the furnace |
| |
| Sr.No. |
Size |
Outer diameter
(in mm) |
Inner diameter
(in mm) |
Wall Thickness
(in mm) |
Ends |
| 1 |
½” 15 N.B. |
- |
- |
2mm |
Both side threaded One side socket |
| 2 |
1/8” |
6mm |
4mm |
- |
Both ends plain |
| 3 |
¼” |
13mm |
- |
1.2mm |
Both side threaded One side socket |
| 4 |
3/8” |
16mm |
- |
1.2mm |
Both side threaded One side socket |
|
|
| |
| |