| Normally in any melting process slagoff is done twice. First at the time when the furnace is half filled and lastly at the time of final slagoff before tapping. METALMIX-X need to be worked into the slag, by means of steel rods to get best efficiency. When mixed before tapping i.e. at the final slagoff after addition of all required ferro alloys wait for 2-3 minutes for the reaction to complete and then used slag coggulant which should be compaitable with-before final slagoff. No further delay should occur before slagoff and tap inorder to avoid oxidation.
METALMIX-X is conveniently packed in 1.0 Kgs to 5.0 Kgs packing depending on the furnace size. So that it became convenient to use.
METALMIX-X is of black colour but do not have to worry as it does not have carbon. At places where aluminium wire/shots and calcium silicide is used during final slagoff is also eliminated as METALMIX-X serves its purpose.
The major benefit of use is threefold. SLAG FLUIDISER, DE-GASSER and DE-OXIDISER resulting into saving in ferro alloys, stop furnace build-up and improve quality of steel produced. |